stainless steel sheet/plate



Hastelloy S is particularly suitable for cyclical heating conditions where components must be capable of retaining their strength, ductility and metallurgical integrity after long time exposure. has excellent thermal stability, low thermal expansion and excellent oxidation resistance at 1093℃. It has good high temperature and thermal fatigue strength. It retains its strength and ductility after aging at temperatures of 427 to 871℃.


Chemical Component

Alloy

%

Ni

Cr

Mo

Fe

Co

C

Mn

Si

W

Al

S

La / P

Hastelloy-S

Min

Balance

14.5

14

-

0.3

0.2

-

0.1

0.01/ -

Max

17

16.5

3

3

0.02

1

0.75

1

0.5

0.01

0.1/0.02


Physical Properties

Density

Fusion Point

Resistivity

CTE

Heat Conductivity

Thermal Diffusivity

Specific Heat

8.75g/cm

1335-1380°C

1.28

11.5 x10E-6

14

3.6 x 10E-6

398


Mechanical Property Under high temperature

Test Sample:1.1-1.6mm

Test Temperature: 1093°C

Tensile Strength

Yield Strength

Elastic Modulus

Elongation

RM N/MM2

RP0.2N/MM2

GPA

%

110

52

212

46

Related Products

  • Incoloy A-286 (UNS S66286 / DIN W. Nr. 1.4980)

  • Incoloy 800(UNS N08800 / W. Nr./EN1.4876)

  • Incoloy 800H/HT

  • Incoloy 825 (UNS N08825/ DIN W. Nr. 2.4858)

  • Incoloy 925/ UNS N09925

  • Hastelloy B-3/UNS N10675 /DIN W. Nr. 2.4600

  • Hastelloy C-4 (UNS N06455, DIN W. Nr. 2.4610)

  • Hastelloy C-22( N06022 , 2.4602)

  • Hastelloy C-276 /UNS N10276 /DIN W. Nr. 2.4819

  • Hastelloy C-2000 (UNS N06200 / DIN W. Nr. 2.4675)

  • Hastelloy G-30 /UNS N06030 / DIN W. Nr. 2.4603

  • Hastelloy N

  • Hastelloy X (UNS N06602 / W.Nr2.4665)